• I want to thank all the members that have upgraded your accounts. I truly appreciate your support of the site monetarily. Supporting the site keeps this site up and running as a lot of work daily goes on behind the scenes. Click to Support Signs101 ...

Liner glue marks on Dibond with UV print

Bewa

New Member
Hello,

We print on pre-cut dibond panels for interior design with a Canon Arizona 1360 GT.
The protective film is difficult to release in one single motion, which results in differences in glossy-ness, which can ben seen very good in solid areas.

I've tried cleaning the surface with pure IPA, 50% IPA, Elix clean (cell phone screen cleaner). This only makes it worse, after cleaning the surface and UV printing on it you can see the wipes of the cleaning in the solid areas.
I tried printing a layer of white first (which is a waste of time and ink when the substrate is already white) and then cmyk, which didn't help.

Anyone knowing the magic solution to get rid of those marks?
Or should I look for another brand of dibond with a film which is easier to release?
 

Attachments

  • 1.png
    1.png
    3.9 MB · Views: 28
  • 3.png
    3.png
    3.2 MB · Views: 27
  • 2.png
    2.png
    3.9 MB · Views: 27

Bewa

New Member
Forgot to mention: i searched for other topics on this matter and also tried:
• Keep wiping with a dry cloth after applying IPA (iso)
• Rolling of the film
• Heating before removing the film
Any combination of these above, none helped...
 

White Haus

Not a Newbie
Seems about right. Which inkset are you using?

We've been using 256 ink on our old 318gl and have never had successful results on ACM due to exactly what you're experiencing. (Light blue/cyan areas always being the worst)

Kind of disappointing to see this is still an issue as we're considering upgrading to a 1360.
 

Bewa

New Member
We're using the 357. Maybe the 358, which is a little more aggressive I heard, gives better results.
Canon sales told me they almost setup each new installation with the 358 instead of the 357 ink.
I'm going to check if I can do some tests at Canon with the 358.
 

White Haus

Not a Newbie
I wonder how much color gamut you actually lose with the 358? I'm not even sure it's an adhesion issue, it's just that their ink is so soft/fragile and lay-down is so thin that it shows absolutely everything.

I suppose the alternative is a harder-curing ink like a lot of competitors, which can lead to chipping.

I have samples printed on 357 and compared to our 256 it's much harder, but I find the quality is still better on our 15 year old 318gl w/ 256 inkset.
 

chinaski

New Member
when I used 258 inks, this never happened (heavier inkset) but with 257 inks it can happen and I'd imagine 256 even moreso. Try different Aluminum Composite products. I switched from 3rd party provider to the original 3A composites "di-lite" and that prevents marks 99% of the time.

I see you're "in Bruges" (great film, btw :D). Just get 3A's "original" product. They're made in Germany so you shouldn't have a problem getting it. "Di-lite" or "Dibond".
 
Last edited:

Grizzly

It’s all about your print!
We had a 660XT about 10 years ago and had these same problems. You can try cleaning with 99% alcohol and make sure you continue to wipe dry and make sure you cover all of it with alcohol. Spray the board and the rag and then wipe consistently. Don't let dry on it's own. We use one of these. https://www.amazon.com/dp/B01E40877Y?ref_=ppx_hzsearch_conn_dt_b_fed_asin_title_5&th=1

All of those problems went away though when we switched to a different flatbed and inkset.
 
Top