Mike Medved
New Member
You are leaning. Water size has only been around for 30 years the ancient Egyptians used blood for gold leaf size but for centuries size was oil based that clay and rabbit glue would be a mess just get some good primer and put 2 or 3 coats down and sand between coats do not brush it on but use spray cans to build it up and your final coat of a good oil base paint can be brushed on because it will hell out smoothly
Can I ask you to clarify? Ok - so - I just paint the wood with a primer (spray acrylic primer? like "the army painter color primer" for example?) A few coats.
Then paint - why use paint and not apply the size to the primer?
Then oil-based size, then the gilding?