• I want to thank all the members that have upgraded your accounts. I truly appreciate your support of the site monetarily. Supporting the site keeps this site up and running as a lot of work daily goes on behind the scenes. Click to Support Signs101 ...

Handprint marks and poor quality with R2000 printing on 3mm PVC

Andrew Hodgson

New Member
I am trying to print onto 3mm PVC using my HP R2000 printer. I am having poor results with PVC. I created a calibrated printer setting with the HP rep when they were here. I am using 12 pass with 110 ink density. I sprayed alcohol to clean the board before printing and brushed it off. I am also having troubles dealing with too much heat that is warping the board while it's printing.

What should I look for or do to get better print quality? Printing on foam board has been fine.
 

Attachments

  • 20260813_102608.jpg
    20260813_102608.jpg
    3.1 MB · Views: 53
  • 20260813_102625.jpg
    20260813_102625.jpg
    2.8 MB · Views: 52

Vassago

Been here a while..
Looks like either poor quality materials, or handling/storage. You cant fix scratches or oil with a quick spray of iso.. Pvc also quite often has static issues.

Check the materials when they arrive.

Check your storage - is it clean and dry.

Check your material handling techniques.. Do they use gloves?

Basically.. Check everywhere your material goes.. If it's placed on a bit of wood before printing, is it smooth, clean, etc.

So many people just throw materials around, then expect perfect results.
 

netsol

Premium Subscriber
i spent MONTHS getting past the static electricity problems when i got my mutoh hybrid
suddenly, sintra was not my favorite material anymore

these people helped quite a bit. very knowledgeable and willing to offer suggestions over the phone

i also bought 3 ionizers from amazon and added that to the input conveyor. the combination of the 2 solutions helped quite a bit.
we would NEVER be large enough to buy substrates in full pallets, which certainly eliminates much of the re-handling problems.
 

Think713

New Member
I am trying to print onto 3mm PVC using my HP R2000 printer. I am having poor results with PVC. I created a calibrated printer setting with the HP rep when they were here. I am using 12 pass with 110 ink density. I sprayed alcohol to clean the board before printing and brushed it off. I am also having troubles dealing with too much heat that is warping the board while it's printing.

What should I look for or do to get better print quality? Printing on foam board has been fine.
Okay so what you wanna do for the warping is go into your profile manager on your IPS computer, and create a profile for your pvc. At the bottom of the main menu when you go into them, if you scroll to the bottom and click the advanced options, you have vaccum settings. Turn them up to the max which is like 1400. Leave your input tension at like 50-75 thats more than enough, but the curing, and heating vaccuum put at like 1400.
Them babies aren't gonna move at those settings. If you get crash warnings from that point, then there is something going on with the vacuums in general. (Or maybe the curing units. I know we technically have 2 faulty curing units that still get hot, but they don't get to their right temps so we have to becareful about what material goes through and how its being fed for said job.) Usually isnt a problem, but it absolutely is with Styrene. Which i hate printing on. Styrene is trash material.

Over the last year or so that I have been running the R2000+ we have, the more ive become familiar with the internal settings. My next move is to find one for magnet material, because we have an issue of the magnet material getting too hot and expanding, and when it cools its bowed on the edges and doesn't go back to original shape. Which makes contour cutting on our colex nearly impossible for accurate door magnets. Very annoying. So I feel your frustration.


We print PVC a lot, and you just have to clean them really really good. You cant see hand oils when cleaning so you cant leave any inch of those things un touched. And try a 90% alcohol rather than a 70.

Hopefully that helps.
 
Last edited:

Think713

New Member
Looks like either poor quality materials, or handling/storage. You cant fix scratches or oil with a quick spray of iso.. Pvc also quite often has static issues.

Check the materials when they arrive.

Check your storage - is it clean and dry.

Check your material handling techniques.. Do they use gloves?

Basically.. Check everywhere your material goes.. If it's placed on a bit of wood before printing, is it smooth, clean, etc.

So many people just throw materials around, then expect perfect results.
I freaking yell at our installers and have to argue with my boss time to time because "where" we have shelves for this material is constantly getting different crap being sat on, or left on, and its always some dirty stuff.. and I'm like you guys... Every time you do this, you ruin this material, and they don't get it. Its beyond annoying. So i moved these materials to inside the print room, and my boss is like... these go on the shelves and im like, until you have a clean shop they stay in here if you want to not lose money on printing.
 

1Trumpet

New Member
Is you setting for heat sensitive material? You can engage the heat deflector handle and divert some of the heat. Also I use a 90% isopropyl alcohol when wiping down the substrate. Then let it dry completely. Then as I precaution I use a static free cloth to wipe it down. Curing temp 160, curing airflow 600, curing height 1.38, heat sensitive curing on, optimizer level 15, dry temp 160, and drying airflow 175. I have had great results with this setting. I always make sure I am wearing gloves when handling as well.
 
  • Agree
Reactions: 1 user

Think713

New Member
Okay so what you wanna do for the warping is go into your profile manager on your IPS computer, and create a profile for your pvc. At the bottom of the main menu when you go into them, if you scroll to the bottom and click the advanced options, you have vaccum settings. Turn them up to the max which is like 1400. Leave your input tension at like 50-75 thats more than enough, but the curing, and heating vaccuum put at like 1400.
Them babies aren't gonna move at those settings. If you get crash warnings from that point, then there is something going on with the vacuums in general. (Or maybe the curing units. I know we technically have 2 faulty curing units that still get hot, but they don't get to their right temps so we have to becareful about what material goes through and how its being fed for said job.) Usually isnt a problem, but it absolutely is with Styrene. Which i hate printing on. Styrene is trash material.

Over the last year or so that I have been running the R2000+ we have, the more ive become familiar with the internal settings. My next move is to find one for magnet material, because we have an issue of the magnet material getting too hot and expanding, and when it cools its bowed on the edges and doesn't go back to original shape. Which makes contour cutting on our colex nearly impossible for accurate door magnets. Very annoying. So I feel your frustration.


We print PVC a lot, and you just have to clean them really really good. You cant see hand oils when cleaning so you cant leave any inch of those things un touched. And try a 90% alcohol rather than a 70.
Also when or if your PVC is coming with a cap sheet (often times they do) DO NOT remove it, until you're ready to print, and still clean that side.

Hopefully that helps.
 

Think713

New Member
Is you setting for heat sensitive material? You can engage the heat deflector handle and divert some of the heat. Also I use a 90% isopropyl alcohol when wiping down the substrate. Then let it dry completely. Then as I precaution I use a static free cloth to wipe it down. Curing temp 160, curing airflow 600, curing height 1.38, heat sensitive curing on, optimizer level 15, dry temp 160, and drying airflow 175. I have had great results with this setting. I always make sure I am wearing gloves when handling as well.
Yes, the curing handle will do you good as well. Even if the material isnt on a heat sensitive setting for the profile, if you increase your passes itll stay in the unit longer, giving you good curing.
 

kaffeinefix

New Member
We print whole sheets on our R2000 daily. We use Windex to clean them. Aggressively. With great results. Spray heavily, wipe down and then clean with a clean micro fibre towel. We do get some warping but it always flattens out after it cools down.
I have gotten scratches like yours as well as hand prints. We always order by the pallet which stays covered until we need it. We have found sheets that have arrived with the scratches and hand prints which don't get discovered until after printing. It's caused many a "conversation" with our vendor which usually work in our favor (again, we order by the pallet).
You can debate Windex versus Alcohol. I've used both and find Windex usually works better but coverage and clean must be pretty aggressive. Windex also removes most of the static.
Think713 has a point in that you can - and should - tweak you heat/vacuum settings. But, as far as scratches and finger prints...it may be coming from the vendor.
 
Top